伊/蒙混层粘土半干法盐酸活化制备活性白土

陈玲玉, 吴炼, 黄克磊, 童张法, 林子珺, 韦藤幼. 伊/蒙混层粘土半干法盐酸活化制备活性白土[J]. 矿产保护与利用, 2016, (2): 48-53. doi: 10.13779/j.cnki.issn1001-0076.2016.02.010
引用本文: 陈玲玉, 吴炼, 黄克磊, 童张法, 林子珺, 韦藤幼. 伊/蒙混层粘土半干法盐酸活化制备活性白土[J]. 矿产保护与利用, 2016, (2): 48-53. doi: 10.13779/j.cnki.issn1001-0076.2016.02.010
CHEN Lingyu, WU Lian, HUANG Kelei, TONG Zhangfa, LIN Zijun, WEI Tengyou. Preparation of Activated Clay by Semidry Method using Mixed-layer Illite/Smectite Clay[J]. Conservation and Utilization of Mineral Resources, 2016, (2): 48-53. doi: 10.13779/j.cnki.issn1001-0076.2016.02.010
Citation: CHEN Lingyu, WU Lian, HUANG Kelei, TONG Zhangfa, LIN Zijun, WEI Tengyou. Preparation of Activated Clay by Semidry Method using Mixed-layer Illite/Smectite Clay[J]. Conservation and Utilization of Mineral Resources, 2016, (2): 48-53. doi: 10.13779/j.cnki.issn1001-0076.2016.02.010

伊/蒙混层粘土半干法盐酸活化制备活性白土

  • 基金项目:

    国家自然科学基金项目

详细信息
  • 中图分类号: TD985

Preparation of Activated Clay by Semidry Method using Mixed-layer Illite/Smectite Clay

  • 采用半干法盐酸活化工艺对伊/蒙混层粘土(I/S)进行活化改性.考察了盐酸浓度、盐酸用量、熟化温度对改性效果的影响,对活化改性工艺进行了优化,并考察了试验制备的活性白土与市售膨润土基活性白土混合使用的效果.结果表明:在盐酸浓度为6%、盐酸用量为粘土质量的30%、盐酸喷雾加料、熟化温度为40℃、熟化时间24 h的条件下,产品活性度(H)达到96.5H+ mmol.kg-1,沥青灯油脱色率(Ra)和菜籽油脱色率(Rr)分别为90.7%和65.2%.XRD分析表明经盐酸活化后,粘土层间距增大,杂质被去除,孔道被疏通.当试验制备的活性白土占混合白土质量的60%以下时,混合白土H>120H+ mmol.kg-1、Ra> 95%、Rr> 80%,与市售活性白土混合使用可降低油脂脱色精炼成本.
  • 加载中
  • 加载中
计量
  • 文章访问数:  1085
  • PDF下载数:  21
  • 施引文献:  0
出版历程
刊出日期:  2016-04-25

目录