Preparation of High Purity Iron Concentrate
-
摘要: 采用阶段磨矿-阶段磁选-脱泥的选矿工艺,处理含铁60.0%、含二氧化硅8.0%的试验样品,可获得含铁70.5%、铁回收率72.92%、含二氧化硅0.67%的高纯铁精矿.
-
-
计量
- 文章访问数: 285
- PDF下载数: 15
- 施引文献: 0
引用本文: | 高洪山. 制备高纯铁精矿的工艺[J]. 矿产综合利用, 2000, (6): 14-16. doi: 10.3969/j.issn.1000-6532.2000.06.004 |