青海某矽卡岩型铁多金属矿选矿试验研究

赵玉卿, 王毓华, 朱琳, 熊馨, 孙晓华, 霸慧文. 青海某矽卡岩型铁多金属矿选矿试验研究[J]. 矿产综合利用, 2015, (5): 34-37,42. doi: 10.3969/j.issn.1000-6532.2015.05.008
引用本文: 赵玉卿, 王毓华, 朱琳, 熊馨, 孙晓华, 霸慧文. 青海某矽卡岩型铁多金属矿选矿试验研究[J]. 矿产综合利用, 2015, (5): 34-37,42. doi: 10.3969/j.issn.1000-6532.2015.05.008
Zhao Yuqing, Wang Yuhua, Zhu lin, Xiong Xin, Sun Xiaohua, Ba Huiwen. Experimental Study on Mineral Processing for a Skarn Type Iron Polymetallic Ore in Qinghai[J]. Multipurpose Utilization of Mineral Resources, 2015, (5): 34-37,42. doi: 10.3969/j.issn.1000-6532.2015.05.008
Citation: Zhao Yuqing, Wang Yuhua, Zhu lin, Xiong Xin, Sun Xiaohua, Ba Huiwen. Experimental Study on Mineral Processing for a Skarn Type Iron Polymetallic Ore in Qinghai[J]. Multipurpose Utilization of Mineral Resources, 2015, (5): 34-37,42. doi: 10.3969/j.issn.1000-6532.2015.05.008

青海某矽卡岩型铁多金属矿选矿试验研究

详细信息
  • 中图分类号: TD952

Experimental Study on Mineral Processing for a Skarn Type Iron Polymetallic Ore in Qinghai

  • 青海某矽卡岩型铁多金属矿含Cu 0.42%、S 5.30%、TFe 35.86%,是以蛇纹石、透辉石、绿泥石为主要脉石矿物的复杂难选铁多金属矿.主要矿石矿物磁铁矿、黄铜矿、黄铁矿、磁黄铁矿间嵌布关系密切,多呈港湾状分布并与脉石矿物包裹、接触,粒度粗细不均,20μm以下含量高,单体解离困难,较难得到合格的精矿产品.根据矿石性质,进行了多种流程试验,最终采用铜硫依次浮选-尾矿选铁流程进行选别,获得了铜精矿品位为16.51%,铜回收率为71.37%;硫精矿品位为29.03%,硫回收率为76.48%;铁精矿品位为63.19%,全铁回收率71.79%,铁精矿含硫0.73%的选矿指标.
  • 加载中
  • 加载中
计量
  • 文章访问数:  593
  • PDF下载数:  15
  • 施引文献:  0
出版历程
刊出日期:  2015-10-01

目录