磁化焙烧-磁选回收某褐铁矿中铁的试验研究

柳林, 王威, 刘红召, 曹耀华, 张博. 磁化焙烧-磁选回收某褐铁矿中铁的试验研究[J]. 矿产综合利用, 2019, (4): 33-37. doi: 10.3969/j.issn.1000-6532.2019.04.006
引用本文: 柳林, 王威, 刘红召, 曹耀华, 张博. 磁化焙烧-磁选回收某褐铁矿中铁的试验研究[J]. 矿产综合利用, 2019, (4): 33-37. doi: 10.3969/j.issn.1000-6532.2019.04.006
Liu Lin, Wang Wei, Liu Hongzhao, Cao Yaohua, Zhang Bo. Research on Recovery of Iron from Limonite by Magnetization Roasting and Magnetic Separation[J]. Multipurpose Utilization of Mineral Resources, 2019, (4): 33-37. doi: 10.3969/j.issn.1000-6532.2019.04.006
Citation: Liu Lin, Wang Wei, Liu Hongzhao, Cao Yaohua, Zhang Bo. Research on Recovery of Iron from Limonite by Magnetization Roasting and Magnetic Separation[J]. Multipurpose Utilization of Mineral Resources, 2019, (4): 33-37. doi: 10.3969/j.issn.1000-6532.2019.04.006

磁化焙烧-磁选回收某褐铁矿中铁的试验研究

  • 基金项目:

    中国地质调查局地质调查项目

    国家自然科学基金项目

    河南省科技攻关项目

详细信息
  • 中图分类号: TD951

Research on Recovery of Iron from Limonite by Magnetization Roasting and Magnetic Separation

  • 某褐铁矿原矿铁品位39.28%,其中褐铁矿矿物含量占73.86%,具有一定的回收价值.以焦煤为还原剂,采用磁化焙烧-磁选的工艺回收其中的铁,试验主要考察了磁化焙烧温度、时间、还原剂加入量、磨矿细度、磁场强度对铁精矿选别指标的影响.确定最佳工艺条件为:磁化焙烧温度800℃,焦煤加入量4%,焙烧时间40min,焙烧样磨矿至-0.037 mm 90%,磁场强度设置192 KA/m进行磁选,最终可获得磁选精矿铁品位59.76%、铁回收率73.31%的良好指标.