微波制备高效脱硫脱硝吸附剂及性能

肖德超, 张军红, 何志军, 湛文龙, 庞清海, 郭庆. 微波制备高效脱硫脱硝吸附剂及性能[J]. 矿产综合利用, 2020, (5): 63-70. doi: 10.3969/j.issn.1000-6532.2020.05.008
引用本文: 肖德超, 张军红, 何志军, 湛文龙, 庞清海, 郭庆. 微波制备高效脱硫脱硝吸附剂及性能[J]. 矿产综合利用, 2020, (5): 63-70. doi: 10.3969/j.issn.1000-6532.2020.05.008
Xiao Dechao, Zhang Junhong, He Zhijun, Zhan Wenlong, Pang Qinghai, Guo Qing. Microwave Preparation and Properties of High-efficiency Desulfurization and Denitrification adsorbent[J]. Multipurpose Utilization of Mineral Resources, 2020, (5): 63-70. doi: 10.3969/j.issn.1000-6532.2020.05.008
Citation: Xiao Dechao, Zhang Junhong, He Zhijun, Zhan Wenlong, Pang Qinghai, Guo Qing. Microwave Preparation and Properties of High-efficiency Desulfurization and Denitrification adsorbent[J]. Multipurpose Utilization of Mineral Resources, 2020, (5): 63-70. doi: 10.3969/j.issn.1000-6532.2020.05.008

微波制备高效脱硫脱硝吸附剂及性能

  • 基金项目:

    国家自然科学基金

详细信息
  • 中图分类号: TD453 TD989

Microwave Preparation and Properties of High-efficiency Desulfurization and Denitrification adsorbent

  • 以粉煤灰、电石渣为原料,在微波场下制备了吸附剂样品,探究反应温度、粉煤灰与电石渣配比、微波功率、辐射时间等因素对脱硫脱硝性能的影响,进而探寻最优的吸附剂制备条件.结果 表明:微波能显著提高吸附剂性能,在粉煤灰与电石渣配比为1:2、微波功率800W、微波辐射时间5 min、反应温度250℃时,脱硫率为99%,脱硝率为96%,脱硫性能略好于脱硝性能,SO2和NO的t 90%脱硫脱硝率达到90%的时间依次为10 min、5 min;运用SEM、XRD、BET等技术对吸附剂进行了表征.XRD结果表明:反应后的样品存在MgSO4、 Ca(NO2)2、 CaSO4的衍射峰.动力学分析表明:高效脱硫脱硝阶段,脱硫符合二级动力学与颗粒内扩散模型共同作用,脱硝符合颗粒内扩散模型;整体脱硫脱硝阶段,脱硫符合颗粒内扩散模型,脱硝符合二级动力学模型.以粉煤灰与电石渣为原料的吸附剂性能优异,有十分重要的环保意义和经济应用前景.