攀枝花微细粒级钛精矿冷固结成型实验研究

侯静, 吴恩辉, 李军, 徐众, 蒋燕, 黄平, 宋馨一, 喻兴亮. 攀枝花微细粒级钛精矿冷固结成型实验研究[J]. 矿产综合利用, 2021, (1): 114-117. doi: 10.3969/j.issn.1000-6532.2021.01.019
引用本文: 侯静, 吴恩辉, 李军, 徐众, 蒋燕, 黄平, 宋馨一, 喻兴亮. 攀枝花微细粒级钛精矿冷固结成型实验研究[J]. 矿产综合利用, 2021, (1): 114-117. doi: 10.3969/j.issn.1000-6532.2021.01.019
Hou Jing, Wu Enhui, Li Jun, Xu Zhong, Jiang Yan, Huang Ping, Song Xinyi, Yu Xingliang. Experimental Study on Cold-bonded Moulding of Panzhihua Micro-size Fraction Titanium Concentrate[J]. Multipurpose Utilization of Mineral Resources, 2021, (1): 114-117. doi: 10.3969/j.issn.1000-6532.2021.01.019
Citation: Hou Jing, Wu Enhui, Li Jun, Xu Zhong, Jiang Yan, Huang Ping, Song Xinyi, Yu Xingliang. Experimental Study on Cold-bonded Moulding of Panzhihua Micro-size Fraction Titanium Concentrate[J]. Multipurpose Utilization of Mineral Resources, 2021, (1): 114-117. doi: 10.3969/j.issn.1000-6532.2021.01.019

攀枝花微细粒级钛精矿冷固结成型实验研究

  • 基金项目:

    国家自然科学基金资助项目

详细信息
  • 中图分类号: TD952

Experimental Study on Cold-bonded Moulding of Panzhihua Micro-size Fraction Titanium Concentrate

  • 以PVA (聚乙烯醇)作为黏结剂,微细粒级钛精矿作为原料,考察了不同黏结剂用量、成型压力和水分含量对微细粒级钛精矿冷固结压力成型生球团机械性能的影响.结果表明:随着黏结剂用量增多,生球团的落下强度和抗压强度越好;成型压力在9MPa时,生球团的抗压强度最优,成型压力在7MPa时,生球团的落下强度最优;水分含量为6%时,生球团的抗压强度和落下强度均达到最优值.综合考虑造球成本,得出微细粒级钛精矿成型工艺最优参数为黏结剂用量0.25%、成型压力7MPa、水分含量6%,所制备的微细粒级钛精矿生球团的抗压强度可达66.88N/球,生球落下强度可达32.8次/球.
  • 加载中
  • 加载中
计量
  • 文章访问数:  290
  • PDF下载数:  73
  • 施引文献:  0
出版历程
刊出日期:  2021-02-01

目录