TiO2对黄金尾砂微晶泡沫玻璃非等温析晶活化能的影响

孙晓刚, 王海龙, 邢军, 邱景平, 程春宏. TiO2对黄金尾砂微晶泡沫玻璃非等温析晶活化能的影响[J]. 矿产综合利用, 2021, (1): 151-156. doi: 10.3969/j.issn.1000-6532.2021.01.026
引用本文: 孙晓刚, 王海龙, 邢军, 邱景平, 程春宏. TiO2对黄金尾砂微晶泡沫玻璃非等温析晶活化能的影响[J]. 矿产综合利用, 2021, (1): 151-156. doi: 10.3969/j.issn.1000-6532.2021.01.026
Sun Xiaogang, Wang Hailong, Xing Jun, Qiu Jingping, Cheng Chunhong. Effect of TiO2 on Crystallization Activation Energy of Gold Tailings Microcrystalline Foam Glass[J]. Multipurpose Utilization of Mineral Resources, 2021, (1): 151-156. doi: 10.3969/j.issn.1000-6532.2021.01.026
Citation: Sun Xiaogang, Wang Hailong, Xing Jun, Qiu Jingping, Cheng Chunhong. Effect of TiO2 on Crystallization Activation Energy of Gold Tailings Microcrystalline Foam Glass[J]. Multipurpose Utilization of Mineral Resources, 2021, (1): 151-156. doi: 10.3969/j.issn.1000-6532.2021.01.026

TiO2对黄金尾砂微晶泡沫玻璃非等温析晶活化能的影响

  • 基金项目:

    十三五国家重点研发课题

    国家自然科学基金面上项目

详细信息
  • 中图分类号: TD982

Effect of TiO2 on Crystallization Activation Energy of Gold Tailings Microcrystalline Foam Glass

  • 以黄金尾砂为主要原料,改变原料中晶核剂TiO2的掺量,制备微晶泡沫玻璃.运用差热分析(DSC)、X射线衍射仪(XRD)等分析手段,研究TiO2掺量对微晶泡沫玻璃析晶与发泡的影响.结果表明,随着TiO2含量的增加,析晶活化能呈现出先减小后增大的规律,当TiO2添加量为3.5%时,析晶活化能较小,为95kJ/mol;同时微晶泡沫玻璃析出的主晶相为硅灰石(CaSiO3),次晶相为钙长石(CaAl2Si2O8);当TiO2添加量为3%~4%时,制备得到的微晶泡沫玻璃具有良好的物理性能;主晶相硅灰石(CaSiO3)不随TiO2的添加改变,并且TiO2能促讲晶相牛长.