中国地质学会岩矿测试技术专业委员会、国家地质实验测试中心主办

低氧低分压环境下泡塑吸附-石墨炉原子吸收光谱法测定化探样品中的痕量金

王 祝, 邵 蓓, 邬国栋, 李明礼. 低氧低分压环境下泡塑吸附-石墨炉原子吸收光谱法测定化探样品中的痕量金[J]. 岩矿测试, 2010, 29(3): 282-286.
引用本文: 王 祝, 邵 蓓, 邬国栋, 李明礼. 低氧低分压环境下泡塑吸附-石墨炉原子吸收光谱法测定化探样品中的痕量金[J]. 岩矿测试, 2010, 29(3): 282-286.
WANG Zhu, SHAO Bei, WU Guo-dong, LI Ming-li. Determination of Trace Gold in Geochemical Samples by Graphite Furnace Atomic Absorption Spectrometry with Polyurethane Foam Preconcentration under Hypobaric Hypoxia Condition[J]. Rock and Mineral Analysis, 2010, 29(3): 282-286.
Citation: WANG Zhu, SHAO Bei, WU Guo-dong, LI Ming-li. Determination of Trace Gold in Geochemical Samples by Graphite Furnace Atomic Absorption Spectrometry with Polyurethane Foam Preconcentration under Hypobaric Hypoxia Condition[J]. Rock and Mineral Analysis, 2010, 29(3): 282-286.

低氧低分压环境下泡塑吸附-石墨炉原子吸收光谱法测定化探样品中的痕量金

Determination of Trace Gold in Geochemical Samples by Graphite Furnace Atomic Absorption Spectrometry with Polyurethane Foam Preconcentration under Hypobaric Hypoxia Condition

  • 针对西藏低氧低分压环境下痕量金的测定,探讨了溶矿介质、解脱时间、吸附温度、Fe3+加入量等对测定结果的影响。确定了最佳测定条件,并较详细讨论了Fe3+在溶矿和吸附过程中的重要作用。方法检出限为0.102 ng/g,测定范围为0.24~300 ng/g,准确度(ΔlgC,n=12)为0.01~0.03,精密度(RSD,n=12)为1.61%~7.33%,很好地解决了西藏地区低氧低分压低温环境下痕量金测定的技术难题。