摘要:
某硫化钼尾矿组成复杂,碳酸盐矿物、萤石、粘土矿物等易浮脉石含量较大,实际生产中回收氧化钼钨矿的成本较高.试验采用Falcon离心机重选预选、离心精矿再浮选的方法,回收硫化钼尾矿中的氧化钼钨.结果表明,采用Falcon重选预选,可提前抛除51.77%的尾矿,重选精矿再经1次粗选3次扫选1次预精选和4次加温精选,可获得含Mo18.92%和WO3 26.79%的氧化钼钨混合精矿,钼钨回收率分别为55.29%、62.51%,达到了降低生产成本的目的.该方法对于伴生低品位白钨矿以及氧化钼矿的回收,具有一定的借鉴意义.
关键词:
-
离心选矿机
/
-
重选
/
-
浮选
/
-
氧化钼
/
-
白钨矿
Abstract:
The cost of bulk flotation for tungsten and molybdenum oxides from a molybdenum sulfide tailings is very high because of the existence of many carbonate minerals and clay minerals.In this paper, the process of gravity concentration-flotation was applied to recover the tungsten and molybdenum oxides from the molybdenum tailings.The results of the tests showed that tungsten and molybdenum bulk concentrate contained 18.92% Mo with the recovery of 55.29% and 26.79% WO3 with the recovery of 62.51% was obtained by a unite technology process, which included gravity concentration with Falcon centrifugal concentrator, the rough concentrate further treated with one stage of roughing, three stages of scavenging, one stage of pre-concentrating and another four stages of heating concentrating.This method provided a reference to the recovery of low-grade white tungsten ore and molybdenum oxide.