山东会宝岭铁矿JCTN提精降渣磁选机选矿试验

王顺, 王兆连, 刘风亮, 李玉永, 张良满, 辛青. 山东会宝岭铁矿JCTN提精降渣磁选机选矿试验[J]. 矿产综合利用, 2017, (4): 73-75. doi: 10.3969/j.issn.1000-6532.2017.04.016
引用本文: 王顺, 王兆连, 刘风亮, 李玉永, 张良满, 辛青. 山东会宝岭铁矿JCTN提精降渣磁选机选矿试验[J]. 矿产综合利用, 2017, (4): 73-75. doi: 10.3969/j.issn.1000-6532.2017.04.016
Wang Shun, Wang Zhaolian, Liu Fengliang, Li Yuyong, Zhang Liangman, Xin Qing. Study on Mineral Processing for Shandong Huibaoling Iron ore JCTN RCG-DDC Permanent Magnetic Separator[J]. Multipurpose Utilization of Mineral Resources, 2017, (4): 73-75. doi: 10.3969/j.issn.1000-6532.2017.04.016
Citation: Wang Shun, Wang Zhaolian, Liu Fengliang, Li Yuyong, Zhang Liangman, Xin Qing. Study on Mineral Processing for Shandong Huibaoling Iron ore JCTN RCG-DDC Permanent Magnetic Separator[J]. Multipurpose Utilization of Mineral Resources, 2017, (4): 73-75. doi: 10.3969/j.issn.1000-6532.2017.04.016

山东会宝岭铁矿JCTN提精降渣磁选机选矿试验

详细信息
  • 中图分类号: TD951

Study on Mineral Processing for Shandong Huibaoling Iron ore JCTN RCG-DDC Permanent Magnetic Separator

  • 为探究JCTN提精降渣磁场机在山东会宝岭铁矿的应用效果,进行了JCTN提精降渣磁选机磁选试验.结果表明:1、采用JCTN提精降渣磁选机用于一段磨后磁选作业,在粒度为-0.074 mm 52%的情况下,可以直接将精矿品位提到66%以上,省掉二段磨以及后续磁选作业;2、将一段磨机处理量从350 t/h提高到500t/h,放粗JCTN提精降渣磁选机给矿粒度,通过与高频筛的配合使用,可以将精矿品位提高到66%以上,节省二段磨矿成本.